Figure 7.

Figure 7

Figure 7

SEM images (AD) of surface roughness at baseline, 24 h, 96 h and 168 h in 4% acetic acid. (A): Baseline SEM photomicrograph of IPS e.max ceramic before immersion in 4% acetic acid (×5000). (B): SEM photomicrograph of IPS e.max ceramic after 24 h immersion in 4% acetic acid (×5000). (C): SEM photomicrograph of IPS e.max ceramic after 96 h immersion in 4% acetic acid (×5000). (D): SEM photomicrograph of IPS e.max ceramic after 168 h immersion in 4% acetic acid (×5000).