. 2022 Jul 25;14(15):3009. doi: 10.3390/polym14153009

Figure 3.

Figure 3

Micrographs of HPP treated biopolymer-based film when applied before casting of films: Cross section of HPP (0, 200, 300, and 400 MPa) treated nisin-soy-protein-isolate film, reprinted with permission from Ref. [30], copyright (2022) Elsevier; Cross section of HPP (0, 200, 400, and 600) treated PVA/CHI/TiO2 film, reprinted with permission from Ref. [36], copyright (2022) Elsevier; Cross section of HPP (at 0, 200 and 400 MPa) treated PLA/AgNPs-3% film, reprinted from Ref. [32].