Skip to main content
. 2022 Jun 15;55(Pt 4):737–750. doi: 10.1107/S1600576722004198

Figure 6.

Figure 6

(a) EBSD IPF-Z map of tungsten, with a black box marking the approximate area scanned during Laue diffraction; (b) recorded Laue image from the scan region centre; (c) Laue image in scattering angle space (the spot size is proportional to the intensity); (d) NN indexing of polycrystals in a Laue image (ten crystals of W are indexed); (e) reconstructed IPF-Z map (pixel size: 1 × 2.5 µm) of the highest matching score for a W crystal in the scanned region along with all the indexed orientations presented in an IPF; (f) principal deviatoric ɛ22 (tensile direction) strain component.