Skip to main content
. 2021 Oct 17;18:37. doi: 10.18502/fid.v18i37.7562

Table 3.

Number (percent) of root fracture modes after pull-out test in the cement groups

Root Fracture Mode Cement P*
Meron glass
ionomer
Zinc
phosphate
Meta
Biomed
Panavia SA
Cement Plus
None 5 (41.7) 8 (66.6) 3 (25) 4 (33.3) 0 . 398
Craze line 4 (33.3) 2 (16.7) 4 (33.3) 2 (16.7)
Craze line and cracks 3 (25) 2 (16.7) 5 (41.7) 6 (50)
Total 12 (100) 12 (100) 12 (100) 12 (100)
*

Chi-square test