Skip to main content
. 2022 Jul 28;12(15):2593. doi: 10.3390/nano12152593

Figure 9.

Figure 9

Permittivity versus measurement frequency dispersion test results for reference HfO2 films as well as nanolaminate stacks grown using amounts of ALD cycles and to the thicknesses indicated by the labels. The capacitor electrode areas were 0.002 mm2.