Skip to main content
. 2022 Jul 30;14(15):3111. doi: 10.3390/polym14153111

Table 2.

Properties of isocyanate adhesive used in this work.

Properties Information
Solids content 98%
Viscosity 150–250 cps/23 °C
pH 6.5–8.5
Pot life mixture Within 60 min
Spread volume 200~250 g/m2
Assembly time Within 10 min
Cold press for a low-density wood 0.69–0.98 MPa
Cold press for a high-density wood 0.98–1.47 MPa
Press time Cold Press 30–45 min depends on wood species, size of lamella, temperature, and spread volume

Source: PT. Polychemie Asia Pasific (Jakarta, Indonesia).