Skip to main content
. 2022 Aug 13;14:163. doi: 10.1007/s40820-022-00893-7

Fig. 5.

Fig. 5

Electrochemical performance of MoO2.0N0.5/NC electrode. Initial charge and discharge cycles of a MoO2.5/NC and b MoO2.0N0.5/NC. c Cycling performance of MoO2.5/NC and MoO2.0N0.5/NC. d Rate cycling performance of MoO2.0N0.5/NC. e Long-term cycling performance at current densities of 10 and 15 A g−1. The insert figures of e shown A the SEM image of MoO2.0N0.5/NC electrode after 10,000 cycles at 10 A g−1 and B the digital picture of separator faced MoO2.0N0.5/NC electrode side. The MoO2.0N0.5/NC cell was disassembled after 10,000 cycles at 10 A g.−1