Table 1.
Comparison of uncoated and coated textile with TiO2 nanoparticle in terms of intrinsic properties of the textile.
| Textiles | Intrinsic properties of the textile | |||||||
|---|---|---|---|---|---|---|---|---|
| Warp resistance N), Mean (SD) | P -value * | Air Permeability (ml/cm 2 /s), Mean (SD) | P- value | Abrasion resistance (kg), Mean (SD) | P -value | Surface wetting resistance (g), Mean (SD) | P -value | |
| Uncoated | 16.19 (3.96) | 0.10 | 21 (1.58) | 0.073 | 204 (1.16) | 0.317 | 0.47 (0.01) | 0.317 |
| Coated with TiO2 | 16.32 (1.62) | 18.80 (1.64) | 501.66 (1.15) | 0.67 (0.01) | ||||
Mann-Whitney Test.