Some bio ceramics' post-implant failure loads3,44–61.

Materials Failure load (kg) Fracture location Ref.
Alumina with high (ρ) 0.13 ± 0.02 Interface 45–48
Bioglass 45S5 2.75 ± 1.80 Within material 49–51
Ceravital (GC) 3.52 ± 1.48 Within material 52–54
Cerabone A/W (GC) 7.43 ± 1.19 Within bone 3 and 55–58