Table 3. Mean Particle Size before and after Freeze Dryinga.
| before
freeze drying |
after
freeze drying |
|||
|---|---|---|---|---|
| sample | mean size (μm) | CV (%) | mean size (μm) | CV (%) |
| S1A | 7.5 | 5.3 | 6.7 | 4.3 |
| S1B | 9.6 | 6.2 | 8.1 | 5.0 |
The CP was 1.5 wt % PVA saturated with IPAc (S1A) or pure 1.5 wt % PVA solution (S1B).