. 2022 Aug 10;2022:1334903. doi: 10.1155/2022/1334903

Table 3.

b value and difference before and after the aging of silicone rubber specimens coated with nano-TiO2 with different concentrations of silicon and aluminum (F = 1951.636, P < 0.05).

Chromatic aberration Concentration
0% 0.05% 0.10% 0.15%
Front 15.22 ± 0.50 7.57 ± 0.48 5.15 ± 0.21 1.09 ± 0.09
After 23.20 ± 0.47 13.40 ± 0.52 9.72 ± 0.21 10.00 ± 0.15
Δb 7.98 ± 0.10 5.83 ± 0.10 4.57 ± 0.10 8.91 ± 0.12