Skip to main content
. 2011 Sep 1;46(17):5680–5689. doi: 10.1007/s10853-011-5519-3

Table 4.

Mechanical properties of pure PAN samples and nanocomposite samples containing 1 wt% of SWCNH with (SU10ta) and without (SU10a) surfactant

Samples Tensile strength RM (MPa) Young’s modulus E (GPa)
PAN 61.5 ± 7.0 2.6 ± 0.4
SU10a 84.4 ± 7.7 3.1 ± 0.3
SU10ta 87.8 ± 6.3 3.4 ± 0.5