. 2010 Jan 1;45(1):158–167. doi: 10.1007/s10853-009-3911-z

Table 3.

Relaxation properties of PTMOx–T6A6T at 25% strain

T6A6T (wt%) G′ (25°C) (MPa) Stress decay (σmax − σ100)/σmax (%) SRn100 − σ10,000)/(σ100 × Δlog t) (% decrease per decade)
Series 1
 PTMO650–T6A6T 44 102 25 6.5
 PTMO1000–T6A6T 34 51 19 6.7
 PTMO1400–T6A6T 27 30 16 5.0
 PTMO2000–T6A6T 21 20 12 6.5
 PTMO2900–T6A6T 16 9 11 4.3