Sample Ferroelectric parameters
P max (μC cm−2) P r (μC cm−2)
BFO–NFO (x = 10%) 6.5874 5.0118
BFO–NFO (x = 30%) 3.4634 2.5253
BFO–NFO (x = 50%) 1.6661 1.4544
BFO–NFO (x = 70%) 0.7161 0.6949