Table 4.
Area (%) of O bonding states measured by XPS on the surface of turned and anodized Ti6Al4V samples.
O bonding state (%) |
|||
---|---|---|---|
Ti4+ - O | Ti3+ - O/C–O | O–H/C=O | |
Control | 39.9 | 43.6 | 16.5 |
Anodized | 52.1 | 15.6 | 32.3 |
Area (%) of O bonding states measured by XPS on the surface of turned and anodized Ti6Al4V samples.
O bonding state (%) |
|||
---|---|---|---|
Ti4+ - O | Ti3+ - O/C–O | O–H/C=O | |
Control | 39.9 | 43.6 | 16.5 |
Anodized | 52.1 | 15.6 | 32.3 |