Skip to main content
. 2022 Aug 22;38(35):10854–10866. doi: 10.1021/acs.langmuir.2c01540

Figure 8.

Figure 8

AFM (first row) and SKPFM (second row) images of the WE43 Mg-based alloy after 10 min of immersion in (a, b) 0.9% NaCl, (c, d) Hank’s, and (e, f) PBS physiological solutions at 37 °C, pH 7.4, and aerated conditions. (g) Height and (h) surface potential histograms that are related to SKPFM images in (b), (d), and (f).