. 2022 Aug 25;11(17):4982. doi: 10.3390/jcm11174982

Table 2.

Roughness values Ra and Rz after aging.

Ra (µm) Rz (µm)
Material * n Mean Max. Min. SD Mean Max. Min. SD
HTML (3Y-TZP) 8 0.230 0.309 0.116 0.064 2.016 3.003 0.850 0.667
STML (4Y-PSZ) 8 0.259 0.330 0.199 0.053 2.099 3.358 1.447 0.604
UTML (5Y-PSZ) 8 0.274 0.334 0.200 0.046 1.946 2.351 1.357 0.334
YML (3–4Y-PSZ) 8 0.222 0.270 0.135 0.046 2.010 3.258 1.119 0.652

* TZP: tetragonal zirconia polycrystal, PSZ: partly stabilized zirconia.