(A) XPS survey spectra for uncoated L605 surfaces treated with and without oxygen plasma, n = 3. Red circle emphasizes location of N 1s peak. (B) XPS survey spectra for uncoated L605, TMS plasma nanocoatings, and TMS+NH3/O2 plasma nanocoatings, n = 3. (C). XPS core-level spectra, n = 3. TMS stands for TMS plasma-nanocoated L605, and TMS+NH3/O2 stands for TMS plasma-nanocoated L605 with NH3/O2 plasma post-treatment.