Skip to main content
. 2022 Sep 9;12:15242. doi: 10.1038/s41598-022-19552-3

Figure 1.

Figure 1

SEM images of piezo catalysts prepared (a) by sonochemistry for 2 h (S1), (b) sonochemistry for 3 h (S2), (c) by solvothermal method at 180 °C for 6 h (S3), (d) by solvothermal method at 245 °C for 6 h (S4), (e) by solvothermal method at 180 °C for 4 h (S5), and (f) by solvothermal method at 245 °C for 8 h (S6).