Table 1.

Drug loading (D–L), encapsulation efficiency (E–E), and diameter (Dv) of GA-loaded microparticles, and span of microparticles prepared by two different methods. (mean ± SD, n = 3).

Method D–L (%) E–E (%) Dv (μm) Span
O/W emulsion 22.3 ± 0.0 74.3 ± 0.9 40.2 ± 16.2 1.11 ± 0.1