Table 3.
Summary of the film thickness data obtained from interferometry for a pure base oil solution. The blue shading indicates that the measurement was conducted after film buildup (i.e., following a period with no change in temperature or rolling speed). The orange shading indicates that the measurement was conducted after a Stribeck Curve measurement was conducted.
Step No | Maximum Thickness [nm] | Minimum Thickness [nm] | Mean Thickness [nm] | Standard Deviation [nm] | Measurement Temperature [°C] |
---|---|---|---|---|---|
A (Zero Point) | 5.0 | −10.0 | 0.3 | 1.5 | 60 |
B (Step 3) | 241.0 | −10.0 | 71.1 | 89.4 | 60 |
C (Step 5) | 233.0 | −6.0 | 54.0 | 83.0 | 60 |
D (Step 7) | 240.0 | −10.0 | 4.5 | 19.8 | 90 |