Comparison of of Drug Release Using Melt Electrospinning and Solution Electrospinning [63].

Sl. No Melt Electrospinning Solution Electrospinning References
1 High crystalline and without a burst phase. Low crystallinity, porous structure, rough, high drug release rate with a burst [63]
2 Diameter of fiber is 1.92 ± 3.31 m when TTCD is 60 mm Diameter fiber of 0.37 ± 0.34 m when TTCD is 200 mm [62]
3 With lower filtration
efficiencies
Higher filtration efficiencies [64]
4 Microfibrous with grid structure Morphology of random nanofiber [59]