Fig. 11.

Fig. 11

a Synthesis procedure and structure of 3D porous Zr-PDI; b illustration of photothermal conversion performance of Zr-PDI*−; c schematic diagram of the PET process between TEA and Zr-PDI, excited state Zr-PDI* is reductively quenched by TEA to afford Zr-PDI*−. Reproduced with permission [111]. Copyright 2018, Springer Nature