Skip to main content
. 2022 Aug 23;4(19):4102–4113. doi: 10.1039/d2na00291d

Fig. 3. Further details on long-pulse VPI depositions (A–C) before or after calcination and dissolution experiments with short-pulse samples (D–F). (A) Swollen pEA in AAO pores after long-pulse AlOx infiltration. (B) Alumina–pEA hybrid material filling pores to different degrees (C) A two-image composite comparing titania films on AAO after calcination. (D) Alumina–pEA hybrid material after 1 h of acetone dissolution. (E and F) Alumina after 10 min dissolution with 5% phosphoric acid with the polymer having been burnt either after (E) or before (F) the dissolution experiment.