Figure 3.
Electrochemical performance in terms of I–V and I–P curves for the Sr0.5Pr0.5Fe0.4Ti0.6O3−δ cell (a), Sr0.5Pr0.5Fe0.3Mg0.1Ti0.6O3−δ cell (b), and Sr0.5Pr0.5Fe0.2Mg0.2Ti0.6O3−δ fuel cell (c) at an operating temperature of 520–420 °C; EIS spectra of Sr0.5Pr0.5Fe0.3Mg0.1Ti0.6O3−δ (d) and Sr0.5Pr0.5Fe0.2Mg0.2Ti0.6O3−δ (e) at the temperature of 520–420 °C in the H2 and air environment; and total and ionic conductivities of Sr0.5Pr0.5Fe0.2Mg0.2Ti0.6O3−δ and Sr0.5Pr0.5Fe0.3Mg0.1Ti0.6O3−δ at 420–520 °C (f).