Skip to main content
. 2022 Sep 30;12:16416. doi: 10.1038/s41598-022-20393-3

Table 4.

Comparison of the mechanical properties of the PMMA-DSNP and PMMA-TiO2NP nanocomposites with those of other nanofiller-based composites.

Material Wear resistance % Coefficient friction resistance % Hardness % Compressive strength (MPa) Ref.
PMMA-DSNP 66.67 88.54 40 145 MPa Present work
PMMA-TiO2NP 61.66 87.18 35 120 MPa Present work
PMMA-Al2O3NP 59.3 25.47 14 110 MPa 40
PMMA-ZrO2NP 58.33- 69.31–64.25% 11 115 MPa 32,47
PMMA-ZrO2NP 55.5% 11 45
DSNP-MDPE 45% 35 39
DSNP-PET 70% 40 35
DSNP-epoxy 71% 27
DSNP-vinyl ester 95 MPa 38