(a) SEM micrographs of wear scars after tribo-corrosion experiments (G0: no GO, G1: 5 ml/l, G2: 10 ml/l, G3: 15 ml/l) (reprinted with permission from Ref. 152), (b) before and after oxidation images of bare and rG-O-coated Cu foils (reprinted with permission from Ref. 153), (c) field trial images of (A–C) virgin silicone fouling release coating formulation and (D–F) PDMS/GO-Al2O3 coating formulation after 90 days in natural marine water (reprinted with permission from Ref. 154).