Skip to main content
. 2022 Oct 6;15(19):6940. doi: 10.3390/ma15196940

Figure 1.

Figure 1

Light microscope images of bonded alumina samples after pressureless treatment in 750 °C with: (a) Bi2O3-5% ZnO interlayer, (b) Bi2O3-10% ZnO interlayer, (c) Bi2O3-15% ZnO interlayer.