Skip to main content
. 2022 Oct 4;5(10):4793–4802. doi: 10.1021/acsabm.2c00505

Figure 4.

Figure 4

Axial force as a function of time for the feeding of the extruder and the melt processing of DAC fibers of 31 or 41% DoM. The 31% DoM fibers had been conditioned at above 90% RH, while the 41% DoM fibers were conditioned at either 30% or above 90% RH. (A) Full data range for the three samples investigated. (B) Extruded filament obtained from melt processing of DAC fibers that had been conditioned at a relative humidity greater than 90%.