Skip to main content
. 2022 Oct 7;7(41):36567–36578. doi: 10.1021/acsomega.2c04530

Table 2. Summary of Parameters Investigated in the Current Work.

parameter modified polyol moisture concentration [ppm] temperature [°C] mixing profile [rpm] catalyst [%]
polyol moisture ≈500/800/1000/2000/3000/4500/6000/13 000 80 100 0.035
catalyst concentration ≈800 80 100 0.035/0.14/0.35/2.1
reaction temperaturea ≈800 80/95/110 100 0.035
mixing regime ≈800 80 30/100/300/750 0.035
a

Both HEURs and prepolymers were investigated in this study.