Skip to main content
. 2022 Sep 22;2(10):2327–2338. doi: 10.1021/jacsau.2c00380

Figure 5.

Figure 5

XRD patterns of calcined Au/f-beta (a) and Au/f-MFI (b) after heat treatment at 500, 600, and 700 °C. Both samples contained 0.48 wt % Au.