Skip to main content
. 2022 Oct 12;12(10):1591. doi: 10.3390/life12101591

Table 1.

Yields 1 (%) and molarities of various P species released as a consequence of Fe3P corrosion in the solution.

Sample Yields (%) Concentration of Various P Species in Solutions (mmolar) 2 Total Molarity (mmolar)
(HPO4)2− (HPO3)2− (P2O7)4− (P2O6)4− [(HPO4)2−] [(HPO3)2−] [(P2O7)4−] [(P2O6)4−]
SEY 71.12 23.40 0.20 5.27 1.20 0.40 0.05 0.10 1.75
F 29.24 54.39 16.37 ND 2.1 2.5 0.3 0.0 4.90
B 48.26 42.69 2.55 6.50 748 413.7 0.95 13.5 1176.1

1 The yields of the corrosion P products of the corrosion reactions were calculated on the basis of the total phosphorus dissolved and by the peak integration method as previously reported [19]. 2 The total molarity of the solution here is the sum of the individual molarities of each of the inorganic P species including (HPO4)2−, (HPO3)2−, (P2O7)4−, (P2O6)4−. The molarities are represented in millimoles. In addition, the labeling of the samples and the solutions descriptions are mentioned in Table 1.