Skip to main content
. 2022 Oct 13;15(20):7109. doi: 10.3390/ma15207109

Figure 20.

Figure 20

The morphological structures of austempered specimens at varying temperatures: (a) 300 °C, (b) 320 °C, (c) 340 °C, and (d) 360 °C [34].