Different grades of austempered ductile iron and the corresponding mechanical properties.

Identification Grade American Standard Grade Based on ASTM89 Ultimate Tensile Strength (Mpa) Strength at Yield (Mpa) Percentage of Elongation (%) Range of Hardness (in Brinell Standard)
A 130-90-09 895.70 620.10 9 269–341
B 150-110-07 1033.50 757.90 7 302–375
C 175-125-04 1205.75 861.25 4 341–444
D 200-155-02 1378.00 1067.95 2 388–477
E 230-185-1 1584.70 1274.65 1 402–522