Table 13.
EDX result of the produced hydroxyapatite optimum parameter (B50/C50) at 900 °C and 500 Pa.
| Elements | Sample (B50/C50) |
||||||||
|---|---|---|---|---|---|---|---|---|---|
| O | Mg | Al | Si | P | K | Ca | Fe | Sr | |
| Concentration (wt%) | 37.041 | 1.154 | 1.119 | 0.884 | 12.153 | 0.073 | 45.503 | 0.313 | 0.118 |
EDX result of the produced hydroxyapatite optimum parameter (B50/C50) at 900 °C and 500 Pa.
| Elements | Sample (B50/C50) |
||||||||
|---|---|---|---|---|---|---|---|---|---|
| O | Mg | Al | Si | P | K | Ca | Fe | Sr | |
| Concentration (wt%) | 37.041 | 1.154 | 1.119 | 0.884 | 12.153 | 0.073 | 45.503 | 0.313 | 0.118 |