Table 1. Fiber Diameters of the Nanofibers Resulted from the Blending of Curcumin and Hydrogenated Castor Oil.

name of the system mean fiber diameter ± SD (nm)
PEO-EC-Co(0.2%)-Cur(1%)@PEO 367.49 ± 98.38
PEO-EC-Co(0.2%)-Cur(3%)@PEO 164.22 ± 37.78
PEO-EC-Co(0.2%)-Cur(4%)@PEO 313.40 ± 96.00
PEO-EC-Co(3%)-Cur(1%)@PEO 144.83 ± 48.05
PEO-EC-Co(5%)-Cur(1%)@PEO 186.21 ± 114.06
PEO-EC-Co(10%)-Cur(1%)@PEO 209.26 ± 41.80
PEO-EC-Co(0.2%)-Cur(1%)@PVP 317.21 ± 79.97
PEO-EC-Co(0.2%)-Cur(3%)@PVP 581.27 ± 222.44
PEO-EC-Co(0.2%)-Cur(4%)@PVP 588.92 ± 26.88
PEO-EC-Co(3%)-Cur(1%)@PVP 190.20 ± 59.42
PEO-EC-Co(5%)-Cur(1%)@PVP 526.44 ± 12.89
PEO-EC-Co(10%)-Cur(1%)@PVP 404.59 ± 45.31