. 2022 Oct 13;15(20):7122. doi: 10.3390/ma15207122

Figure 11.

Figure 11

Recrystallized (blue), substructure (yellow), and deformed (red) grains in TC4 alloy: (a,c) Hot-rolled; (b,d) 930 °C/15 min, WQ + 560 °C/2 h, FC.