Tensile strength and modulus of the UHMWPE/HDPE SrCs prepared at different packing time (a), the numerically calculated temperature in the cavity after the filling stage (b), the numerically calculated viscosity of the matrix in the cavity after the filling stage (c), and the density of the matrix after the packing stage (d).