Skip to main content
. 2022 Oct 11;14(20):4258. doi: 10.3390/polym14204258

Table A3.

Compression test porosity results of the first five specimens, compressed at 210 °C and 10 min of dwell time, with various compaction pressures (sample 1 with 10 MPa, 2 with 8 MPa, 3 with 6 MPa, 4 with 4 MPA, 5 with 2 MPa).

Porosity Volume Fraction (%)—Data
Sample 1 2 3 4 5 St. Deviation (%) Average (%)
1 0.49 0.56 4.21 0.33 0.21 1.71 1.16
2 0.74 1.06 0.4 0.75 2.34 0.75 1.06
3 0.53 0.55 0.39 0.37 4.6 1.85 1.29
4 3.85 5.78 4.01 4.56 2.38 1.23 4.12
5 3.76 6.79 8.46 6.41 1.84 2.63 5.45