Compression test porosity results of the second two specimens, compressed at 200 °C and 10 min of dwell time, with various compaction pressures (sample 1 with 10 MPa, 2 with 8 MPa, 3 with 6 MPa, 4 with 4 MPA, 5 with 2 MPa).

Porosity Volume Fraction (%)—Data
Sample 1 2 3 4 5 St. Deviation (%) Average (%)
1 0.22 0.16 0.26 0.16 0.49 0.14 0.26
2 0.86 0.53 0.48 0.36 0.83 0.22 0.61