Table 1.
Sample | D + G-Mode | Layer Thickness, nm | Estimated Porosity, % | ||
---|---|---|---|---|---|
I, cps∙105 | RSD, % | SEM | TEM | ||
MFGO | 4.33 | 9.5 | 45 ± 5 | - | 10 |
CNTGO@MFGO | 1.71 | 8.7 | 37 ± 5 | 31 ± 3 | 50 ± 10 |
C60(OH)26–32@MFGO | 3.17 | 22.4 | 30 ± 4 | 20 ± 3 | 5 ± 5 |
Sample | D + G-Mode | Layer Thickness, nm | Estimated Porosity, % | ||
---|---|---|---|---|---|
I, cps∙105 | RSD, % | SEM | TEM | ||
MFGO | 4.33 | 9.5 | 45 ± 5 | - | 10 |
CNTGO@MFGO | 1.71 | 8.7 | 37 ± 5 | 31 ± 3 | 50 ± 10 |
C60(OH)26–32@MFGO | 3.17 | 22.4 | 30 ± 4 | 20 ± 3 | 5 ± 5 |