Fig. 6. Electrocatalytic performance.

Fig. 6

RDE mass activity (a), and specific activity (b) of the STG-assisted Pt-IMCs catalysts and TKK-30 wt% Pt/C. The Pt loading in RDE tests were in the range of 11~13 µg cm–2. c Correlation between specific activity and calculated surface strain of the five L10 PtM catalysts and Pt/C. The error bars in a, b, and c were obtained after three parallel experiments. d Mass activity loss of the MEAs made with cathode catalysts of STG-assisted PtCo, Umic-30 wt% PtCo, TKK-30 wt% Pt/C, and TKK-30 wt% Pt/C-700 after 30,000 cycles’ ADT. e H2-air polarization curves and power density plots of the MEAs made with cathode catalysts of STG-assisted PtCo, Umic-30 wt% PtCo, TKK-30 wt% Pt/C, and TKK-30 wt% Pt/C-700. For all MEA, the cathode and anode loadings were controlled to be 0.1 and 0.025 mgPt cm–2, respectively. Test conditions: 80 °C, 100% RH, 150 kPaabs, outlet H2-air at high stoichiometries (H2 and air flow rates were fixed at 0.5 and 2.0 L min–1, respectively). f Voltage loss at 0.8 A cm–2 of the MEAs made with cathode catalysts of STG-assisted PtCo, Umic-30 wt% PtCo, TKK-30 wt% Pt/C, and TKK-30 wt% Pt/C-700 after 30,000 cycles’ ADT.