Table 3. Pseudo-First-Order Rate Constants (min–1) for MO, MB, Rh B, and NR Dye Degradation under Solar Light Irradiation.

  k (10–3 min–1)
photocatalyst MO Rh B MB NR
g-C3N4 9.7 10.8 16.4 12.5
Cs0.33WO3 4.4 1.6 7.8 10.4
g-C3N4@Cs0.33WO3 19.6 19.5 40.3 31.5