a),b) GPC molecular weight distributions of DMA/NHS polymer library polymerised at a monomer concentration of a) 0.5m, [DMA]/[NHS] = 9:1 (Supporting Information, Table S3) and b) 1m, [DMA]/[NHS] = 9:1 and 8:2 (Supporting Information, Table S5). c) FTIR on crude polymers from 0.5m polymerisation (Supporting Information, Table S6) after functionalization with DBCO-NH2 and Man(OAc)-N3 showing almost full functionalization. d) GPC molecular weight distributions of DP40 polymers before and after functionalization with DBCO-NH2 and PEG7-N3 (Supporting Information, Table S4). All polymers containing NHS were reacted with butyl amine before running the GPCs.