Table 3. Failure mode distribution in each experimental group after push-out test.
Groups | ACD | ACP | M | CD | CC | CP |
---|---|---|---|---|---|---|
AH Plus/RelyX ARC | 8 | 15 | 8 | 24 | 3 | 2 |
AH Plus/RelyX U200 | 28 | 10 | 8 | 12 | 2 | - |
Bio-C Sealer/RelyX ARC | 20 | 21 | 6 | 12 | 1 | - |
Bio-C Sealer/RelyX U200 | 13 | 10 | - | 35 | 2 | - |
Sealer Plus BC/RelyX ARC | 38 | 3 | 5 | 14 | - | - |
Sealer Plus BC/RelyX U200 | 29 | 4 | 1 | 26 | - | - |
Total | 136 (37.8%) | 63 (17.5%) | 28 (7.8%) | 123 (34.1%) | 8 (2.2%) | 2 (0.6%) |