Table 1.

The crystallite size of the prepared LDH and LDH/MO samples.

Samples Crystallite size (nm)
Before adsorption After adsorption
As prepared 2.77 4.59
LDH-calcination 200 °C 3.45 4.17
LDH-calcination 400 °C 5.65 6.92
LDH-calcination 600 °C 8.16 19.82