. 2022 Nov 4;15(21):7795. doi: 10.3390/ma15217795

Figure 3.

Figure 3

Diagram of the heat treatment regime during the hard-facing: 1—slow heating in the oven; 2—holding at the preheating temperature (T = 230 °C, t = 2 h); 3—hard-facing; 4—returning to the furnace (T = 230 °C, t = 1 h); 5—slow cooling together with the oven.