. 2022 Nov 4;14(21):4729. doi: 10.3390/polym14214729

Table 2.

The results of the TG and DTG curve analyses of P1–P5.

Type of Polymer Nanoparticle System T1
(°C)
Rate of Mass Loss 1 (% min−1) T2
(°C)
Rate of Mass Loss 2 (% min−1) T3
(°C)
Rate of Mass Loss 3 (% min−1) TOnset
(°C)
TEndset
(°C)
Res. at 760 °C
(%)
T1.0wt%
(°C)
P1 52.3 0.59 274.0 0.50 397.9 9.45 343.0 410.5 6.88 31.8
P2 51.0 0.68 274.9 0.46 396.2 9.68 356.3 408.6 4.38 33.1
P3 48.8 0.64 293.3 0.45 395.7 9.54 361.5 410.3 7.10 31.3
P4 52.0 0.67 289.7 0.50 395.9 9.38 357.3 395.9 7.15 31.7
P5 53.2 0.65 288.1 0.42 397.6 9.99 372.3 411.9 7.10 31.8