. 2022 Nov 14;264:126096. doi: 10.1016/j.energy.2022.126096

Table 7.

Observational findings from the treatment of BMW in LDPE + HDPE solvent.

S. No. Sample No. The temperature of dissolution initiation Peak Temperature Remark
13 12 115–120 140 Slightly cloudy supernate
14 13 115 130 dissolve in oil but do not settle down
15 14 115, speed up after 130 150
16 15 115 130