XRD patterns of 45S5 bioglass powders (blue curve), 3D printed scaffold after sintering at 1100°C for 2 h (red curve). The peaks of the Na6Ca3Si6O18 phase and Na2Ca4(PO4)2Si2O4 phase were marked by ● and ○, respectively.